Assembly glue use guide
1. Bonded wood moisture content: 6-10%.
2. The coating uniformity of the rubber layer does not exceed ±0.15mm error.
3. The material to be bonded should be pressurized after bonding. The pressure should be adjusted according to different materials, low density material 6-10kg/cm2, high density material 12-18 kg/cm2.
4. When pressing, it can be adjusted according to the ambient temperature.
5. The bonding material should be placed in the body for 24 hours before being mechanically processed.
6, please operate in the environment above 50C. Scope of application: This glue belongs to high solid content, fast adhesive, general furniture, woodworking hoe, Pauli board, melamine board, wood brick, stone, decorative paper, leather, linen, paper, etc.